Facade joint renewal starts where the filler, which has to flex as the building moves, has worn out. Without scaffolding, descending on ropes, we cut out sealant that has cracked or torn away between panels, in the expansion gaps between blocks and around window frames; we prepare the joint from scratch and close it with new filler.

Water that gets in through an open joint often leaves its mark several storeys lower down. That is why we start the survey not from the flat where the leak shows but from the joint itself.

Roped technician working on the panel-clad facade of a tall apartment block

Why Does a Facade Joint Need a Flexible Filler?

A building moves as it warms and cools during the day, under wind load and in an earthquake. A facade joint is the gap left for that movement, and the filler inside has to be able to open and close with it.

A facade joint closed with hard mortar or the wrong sealant comes away at the edge in the first winter. When the water that gets in through the gap freezes, it opens the gap a little wider.

Comparison of a facade joint and a tile joint
TopicFacade jointTile joint
PurposeSeparates two surfaces that moveCloses the narrow gap between ceramic tiles
FillerElastic sealant; bonds to the two side facesCement-based, hard grout
MovementOpens and closes with heat, wind and earthquakesNot expected to move
Who does itThe facade team working at heightInterior and tiling tradespeople

Short Answers About Facade Joints

How is facade joint renewal done?

The old filler is cut along both edges and removed, and the sides of the joint are cleaned and dried. A foam backing rod is placed to set the depth, a primer is applied to the sides and a suitable sealant is applied without leaving gaps. Finally the surface is tooled smooth. On multi-storey buildings, all of this is done along the joint line by technicians on ropes.

How is facade joint filler renewed, and must the old one be removed?

It must. New sealant applied over the old filler bonds to the aged layer and comes away together with it. For a lasting result, the old filler and the residues on the sides are cleaned off completely and the joint is prepared from scratch.

Why does an expansion joint open up, and is it dangerous?

The expansion gap is left so that the building can move; what opens is usually the filler inside it. Sun, frost and repeated movement harden the sealant and pull it away from the edges. Water entering through an open joint can reach the reinforcement and the insulation; if a clear change in the width of the joint is seen, a structural engineer needs to assess it.

Can the facade be painted after the joint has been renewed?

Polyurethane and MS polymer sealants can be painted over once they have cured. Paint does not adhere to silicone sealant. If painting is planned, we choose the product accordingly and do the two jobs one after the other with the same rope rigging.

Expansion Joints and Facade Movement Joints

Although the two types of joint are closed with similar materials, their functions differ, and they need different detailing when renewed.

An expansion joint is the gap left from foundation to roof between two parts of a building that work independently of each other; it is also called a seismic joint. On the facade this gap is closed with a wide sealant fill or a cover profile.

A facade expansion joint, on the other hand, takes up thermal movement between precast panels, stone or cladding joints. It is narrower, but because there are so many of them, the total length on the facade is high.

The width of a joint is set in the building’s design, according to the relevant regulations and standards (for example TS 500). When renewing, we do not narrow this gap; we close it with a material suited to the existing width.

Plan section of an expansion gap: two blocks, the joint between them and the layers of the filler.
  1. 1Cover profile: Only on wide seismic joints; covers the gap from outside.
  2. 2Sealant: Bonds to the two side faces and flexes as the building moves.
  3. 3Primer: Strengthens the bond of the sealant to the side faces.
  4. 4Backer rod: Sets the depth and stops the sealant bonding to the bottom.

Renewing Facade Joint Filler: Choosing Sealant and Profile

The life of the filler begins with a product suited to the movement of the joint and the type of surface. At the survey we identify the type of the old filler and choose a compatible product.
Filler materials used in facade joints
MaterialWhere it is usedMovement capabilityNote
Polyurethane (PU) sealantConcrete panels, expansion gapsHighCan be painted over; protecting it from the sun with paint is recommended
MS polymer (hybrid) sealantPanel, stone and metal junctionsHighCan be painted; compatible with a wide range of surfaces
Silicone sealantGlass, aluminium and metal junctionsVery highCannot be painted over; on natural stone a special non-staining type is chosen
Acrylic sealantInteriors, static cracksLowNot suitable for movement joints on a facade
Expansion joint cover profileWide seismic jointsDepends on the type of profileFor gaps too wide to be closed with sealant

A mistake we often come across when choosing sealant for external walls is interior acrylic applied to a concrete panel joint. It cracks within a year or two and the whole line has to be cut out again.

Facade Joint Renewal Step by Step

Applying new filler over the old only postpones the problem by a few months. The joint is prepared from scratch every time.
  1. 1

    Removing the old filler

    The sealant is cut along both edges and pulled out, the residue on the side faces is scraped off, and the joint is cleaned down to the bottom.

  2. 2

    Dryness check

    Sealant will not bond to a wet surface. After rain we wait for the joint to dry completely.

  3. 3

    Backer rod

    Closed-cell foam backer rod is pressed in to the level that sets the depth. Sealant is generally applied to a depth of half its width.

  4. 4

    Primer and masking

    The manufacturer’s primer is applied to the side faces and the joint edges are protected with tape.

  5. 5

    Sealant

    The filler is applied with a gun without leaving voids; it bonds only to the two side faces and does not touch the bottom.

  6. 6

    Tooling

    The surface is pressed with a spatula to a concave profile, and the tapes are removed before the sealant cures.

Roped technician applying backing rod and sealant to a panel joint on a tile-clad facade

Precast Panels, Gaps Between Blocks and Window Surrounds

Most of the joints we renew on tall buildings are found in these four places.
  • Precast and GRC panel joints

    On panel facades every junction is a joint; the vertical and horizontal lines can add up to hundreds of metres on one building.

  • Expansion gaps between blocks

    In multi-block developments such as housing estates, hospitals and schools, the wide gap running from roof to ground between the blocks.

  • Around window frames and sills

    The filler between a window and the wall is one of the most common sources of facade leaks.

  • Where different materials meet

    Lines where stone cladding meets concrete or a metal panel meets render; the two materials expand at different rates.

We cover the silicone joints between panes of glass on our curtain wall page. If the concrete around a joint has crumbled, the repair is carried out as part of facade crack repair.

As well as housing estates and public buildings in Ankara, we send a team for panel facades outside the province too; the equipment comes to site with us.

What Do We Look At in a Facade Joint Survey?

At the end of the survey you receive the joint length, the type of filler we recommend and the work schedule in writing.
  1. We note the flat and room where the leak shows.
  2. We check the joints from top to ground, with binoculars or by descending on ropes.
  3. We test the type and adhesion of the old filler on site.
  4. We measure the width of the joint and work out the length.